Table 3 Mass of sapphire glass before and after the corrosion resistance test (conditions: 450 °C, 102 MPa, mineralizer concentration 2.0 mol%, and 6 h)

From: Temperature dependent control of the solubility of gallium nitride in supercritical ammonia using mixed mineralizer

Mineralizer Mass of sapphire glass before experiment (g) Mass of sapphire glass after experiment (g)
NH4F 1.1998 1.1814
NH4Cl 1.1930 1.1894