Skip to main content

Table 3 Grinding condition and particle size of water-dispersible Fmoc-Ala-OH nanoparticlesa

From: Development of a method for environmentally friendly chemical peptide synthesis in water using water-dispersible amino acid nanoparticles

Entry

Detargent agent

Bead Size [mm]

Particle Size [nm]

1

0.4% Triton X-100 solution

0.5

292 ± 119

2

0.2% Triton X-100 solution

0.5

217 ± 89

3

0.2% Triton X-100 solution

1.0

362 ± 157

4

0.1% Triton X-100 solution

1.0

484 ± 225

5

0.01% Triton X-100 solution

1.0

2581 ± 954

  1. aAn aqueous dispersion of nanoparticulate Fmoc-Ala-OH was prepares by grinding using a planetary ball mill. An agate jar was charged with precleaned zirconium oxide beads, Fmoc-Ala-OH, and detergent solution. The batch was rolled for 3 hr. After grinding, the beads were removed by filtration with water.