Figure 9From: Characterization of deposits formed on diesel injectors in field test and from thermal oxidative degradation of n-hexadecane in a laboratory reactor(a) TPO profile of HPDI deposits. (b) TGA-MS profile of CO2 and H2O evolved from the oxidation of carbon and hydrogen species in HPDI deposits from 100–1000°C.Back to article page