Table 2 Results of non-isothermal TG/DTG of the PS/BCHMX nanofiber membrane, polystyrene membrane, and pure at a heating rate of 10 K min−1

From: Spun of improvised cis‐1,3,4,6‐tetranitrooctahydroimidazo‐[4,5‐d]-Imidazole (BCHMX) in polystyrene nanofibrous membrane by electrospinning techniques

Type

TG curve

DTG curve

β/oC min−1

To/oC

Mass loss/%

Tp/oC

Toe/oC

Polystyrene nano-fiber membrane

10

335.1

99.5

381.2

416.7

Polystyrene polymer

377.9

99.9

405.2

421.7

PS/BCHMX (Peak I)

225.0

57.9

233.7

240.7

PS/BCHMX (Peak II)

309.8

40.9

386.8

424.5

BCHMX (Peak I)

202.1

53.3

211.1

217.8

BCHMX (Peak II)

233.6

45.3

241.8