Fig. 3From: On the role of composition and processing parameters on the microstructure evolution of Ti-xMo alloysBackscatter SEM micrographs for two deposited specimens a 2.4 MJ in−3 (~ 149 kJ cm−3) and b 7.4 MJ in−3 (~ 448 kJ cm−3)Back to article page