From: Removal of alachlor from water by catalyzed ozonation on Cu/Al2O3honeycomb
Catalyst | BET surface area(m2g-1) | Pore volume(cc g-1) | Pore diameter(A) |
---|---|---|---|
1 wt.% Cu-Al2O3 | 235.1 | 0.7214 | 122.8 |
5 wt.% Cu-Al2O3 | 205.1 | 0.6280 | 122.58 |
10 wt.% Cu-Al2O3 | 171.9 | 0.5298 | 123.3 |
15 wt.% Cu-Al2O3 | 147.7 | 0.4839 | 128.5 |